Abstract

A new process for the production of pigments suitable for use in paper laminates has been developed in which a metal oxide is treated with a water-soluble salt of zinc and a phosphate or phosphoric acid and subsequently with an alkali metal aluminate in such a manner that there is deposited on the metal oxide a coating containing zinc and phosphate ions together with aluminium ions. The pH of the dispersion following the metal oxide is maintained at a value not exceeding 8.0 during precipitation. A particularly useful pigment is produced which has a coating containing zinc ions in an amount of 0.5 to 5% by weight as ZnO, phosphate ions in an amount of 0.2 to 3% as P 2 O 5 and aluminium ions in an amount of 0.5 to 5% expressed as Al 2 O 3 on the weight of TiO 2 .

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 30.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A process for the production of a pigment comprising forming an aqueous dispersion of a titanium dioxide pigment containing a water soluble salt of zinc and a phosphate or phosphoric acid, adding to the dispersion an alkaline solution of an alkali metal aluminate to precipitate a coating containing zinc and phosphate ions and maintaining the pH of the dispersion during precipitation of the coatings at a value not exceeding 8.0.

  2. Claim 2Depends on #1

    A process according to claim 1 in which the amount of the said salt of zinc present is such as to provide 0.5% to 5% by weight zinc expressed as ZnO on the weight of TiO 2 .

  3. Claim 3Depends on #1

    A process according to claim 1 in which the amount of phosphate or phosphoric acid present is such as to provide from 0.2% to 3.0% of phosphate expressed as P 2 O 5 on weight of TiO 2 .

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗