Method and apparatus for producing superconducting joints
Abstract
A method for joining two or more superconducting wires each comprising a bundle of filaments of tin (Sn) and niobium (Nb) contained within a binder metal with a superconducting joint. The filaments on the ends of the wires to be joined are first exposed by etching the binder metal away with acid and then the exposed filaments are intertwined. The exposed filaments are then sealed in a copper-enriched chamber and heated to a temperature and for a time sufficient for the Sn and Nb to diffuse together and form Nb 3 Sn at their interface. Preferably, the filaments are sealed by forming a tubular jacket, placing the tubular jacket over the exposed filaments and the wire ends adjacent thereto, and swaging the ends of the tubular jacket to the wire ends adjacent the exposed filaments. The jacket can be formed by obtaining wire comprising a thick outer layer and a thin inner layer of copper separated by a thin barrier layer of a material chosen from the group consisting of vanadium, niobium, and tantalum, or the like, all disposed over a tin core, cutting the wire to desired jacket lengths, heating the jacket lengths of the wire to melt the tin cores thereof, and blowing the melted cores f
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 11.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
In unalloyed wires for superconducting said wires comprising a bundle of filaments of tin (Sn) and niobium (Nb) contained within a binder metal, a method of joining two wires with a superconducting joint comprising the steps of: a) exposing the filaments on the ends of the wires to be joined; b) intertwining the exposed filaments; c) sealing the exposed filaments in a copper-enriched chamber; and, d) heating the chamber to a temperature and for a time sufficient for the Sn and Nb to diffuse together and form Nb 3 Sn at their interface.
- Claim 2Depends on #1
The method of forming a superconducting joint between two wires of claim 1 wherein said step of heating the chamber to a temperature and for a time sufficient for the Sn and Nb to diffuse together and form Nb 3 Sn at their interface
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗