Patents
US 5,108,570 A#82712 Most CitedExpiredUnited States (USPTO)Utility

Multistep sputtering process for forming aluminum layer over stepped semiconductor wafer

164Forward Citations (#82712 Global)
4.8/yrCitation Velocity (#303925 Global)
20.58Citation PageRank (#318216 Global)
4Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A multistep aluminum sputtering process is disclosed wherein aluminum is sputtered onto the surface of a semiconductor wafer and low areas between closely spaced apart raised portions on the wafer, such as closely spaced apart steps, narrow trenches, or small diameter vias, are completely fulled in by the sputtered aluminum. This results in the formation of an aluminum layer which is not thinned out in such low areas, and which has a surface which ranges from substantially planar to a positive slope, such as shown at 24' and 26' in FIG. 2. The first step is carried out by sputtering from about 200 to about 2000 Angstroms of aluminum while the wafer temperature is within a range of from about 50° C. to about 250° C. and the sputtering plasma is at a power of from about 1 to about 16 kilowatts. The power level range is then changed to from about 14 to about 20 kilowatts, a DC or AC bias is applied to the wafer, and aluminum is then sputtered either for an additional time period of about 20 to about 40 seconds or until the wafer temperature reaches 500° C., whichever occurs first, in a second step. Then the back side of the wafer is contacted by a thermally conductive gas to c

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 164.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A sputtering process for forming an aluminum layer over a stepped semiconductor wafer in a splattering chamber which comprises: (a) sputtering from about 200 to about 2000 Angstroms of aluminum from a target onto said wafer in a first deposition step while maintaining a power level on said target of from about 1 kilowatt to about 16 kilowatts; (b) providing a target power level of at least about 14 kilowatts and sputtering aluminum for an additional 25 to 45 seconds or until the wafer temperature reaches about 500° C., whichever occurs first, during a second deposition step, while applying a

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗