Patents
US 5,100,728 A#438892 Most CitedExpiredUnited States (USPTO)Utility

High performance pressure sensitive adhesive tapes and process for making the same

74Forward Citations (#438892 Global)
2.2/yrCitation Velocity (#1727550 Global)
10.68Citation PageRank (#951250 Global)
8Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A pressure sensitive adhesive tape comprises a carrier layer having a thickness of 0.25 to 2.0 millimeter and comprising an electron beam cured pressure sensitive adhesive matrix, 10 to 20% by volume low density microspheres and at least one pigment in an amount sufficient to color the tape. Preferably, fumed silica is present in an amount up to 5% by weight. The tape preferably has a kin layer on each side of the carrier layer. The skin layer has a coating thickness of 25 to 125 g/m 2 and comprises a pressure sensitive adhesive matrix free of rigid, low density microspheres. The process comprises first preparing an adhesive composition containing electron beam-curable adhesive polymer matrix, fillers and solvent. The composition is introduced and conveyed through a twin screw extruder. In the extruder, solvent is removed in one or more solvent removal units, and a solvent-free composition is extruded as the carried layer. Skin layers may be co-extruded with the carrier layer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 74.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A pressure sensitive adhesive tape having a carrier layer comprising an electron beam-cured pressure sensitive adhesive polymer matrix, form about 5% to about 70% by volume low density microspheres and at least one ultraviolet light absorbable pigment in an amount of at least 0.2 percent by weight, wherein the pressure sensitive adhesive tape exhibits substantially no decrease in creep as compared to the same pressure sensitive adhesive tape without pigment.

  2. Claim 2Depends on #1

    An adhesive tape as claimed in claim 1 wherein the pressure sensitive adhesive polymer matrix is acrylic based and the creep at 70° C. is at least about 166 hours.

  3. Claim 3Depends on #1

    An adhesive tape as claimed in claim 1, wherein the carrier layer has a thickness of from about 0.25 to about 4.0 mm.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗