Industrial asphalts
Abstract
Disclosed is a method of producing an industrial asphalt from a bituminous material. One preferred embodiment comprises mixing together without air-blowing: a. a feed material comprising a bituminous material having a viscosity of at least 50 centistokes at 350° F. and wherein said feed material forms a single phase when mixed with 5 percent of 85 percent phosphoric acid; and b. from about 0.1 to 20.0 percent by weight of phosphoric acid, said mixing being done at a temperature in the range of 351° to 600° F., whereby the softening point of the feed is substantially increased and the penetration is significantly decreased. A second preferred embodiment comprises heating at an elevated temperature a mixture comprising: 1. from about 0.1 to 20.0 percent by weight green phosphoric acid, and 2. a bituminous material to make up 100 percent by weight, said bituminous material comprising asphalt.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 22.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A one-step method of producing an industrial asphalt from a bituminous material which comprises mixing together without air-blowing either before, during, or after said mixing; a. a feed material comprising a bituminous material having a viscosity of at least 50 centistokes at 350° F. and wherein the feed bituminous material forms a single phase when mixed with 5 percent of 85 percent phosphoric acid; and b. from about 0.1 to 20.0 percent by weight of phosphoric acid having an H 3 PO 4 equivalent of less than 100 percent, said mixing being done at a temperature in the range of 351° to 600°
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗