Patents
US 5,096,497 A#5136365 Most CitedExpiredUnited States (USPTO)Utility

Cement composition

17Forward Citations (#5136365 Global)
0.5/yrCitation Velocity (#15146880 Global)
5.16Citation PageRank (#3150702 Global)
10Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A hardened cement is prepared by mixing together two slurries, one comprising water and a cement component and the other comprising water, beta anhydrite and calcium oxide and or calcium hydroxide. According to the invention the cement component of the first slurry comprises ferrite and C 12 A 7 or A 7 A--CX 2 (where X is a halogen atom) and a reactive source of silica.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 17.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A two part composition for use in making a hardened cement, the composition comprising first and second slurries, the first slurry comprising water, a reactive source of silica and a cement component, the cement component comprising the phases ferrite and C 12 A 7 or ferrite and C 11 A 7 CX 2 (where X is a halogen), the phases making up at least 50% by weight of the cement component, the reactive source of silica being present in a weight ratio of 0.1 to 0.6:1 of the cement component, the second slurry comprising water, beta anhydrite, and a calcium compound selected from the group consis

  2. Claim 2Depends on #1

    A composition according to claim 1, wherein the ferrite and C 12 A 7 or C 11 A 7 CX 2 make up 65 to 85% by weight of the cement component of the first slurry.

  3. Claim 3Independent Claim

    A composition acco

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 17 total)

PatentTitleYearCitations
US 7,708,825 B2Sialite binary wet cement, its production method and usage method20104
US 2008202415 A1Methods and systems for addition of cellulose ether to gypsum slurry—21
EA 022,450 B1Improvements in or relating to cementitious compositions—0
US 8,627,769 B2Cementitious compositions20141
US 8,413,584 B2Cementitious compositions20135
US 6,406,534 B1Rapid hardening, ultra-high early strength portland-type cement compositions, novel clinkers and methods for their manufacture which reduce harmful gaseous emissions200225
US 6,502,636 B2Methods and compositions for grouting heat exchange pipe200338
WO 2004/058662 A1A two-component wet cement, process and application thereof—8
US 6,113,684 ARapid hardening, ultra-high early strength Portland-type cement compositions, novel clinkers and methods for their manufacture which reduce harmful gaseous emissions200062
ES 2,154,571 A1Materials possessing mechanical resistance and low leaching ability are obtained from mining and industrial residues—0
RU 2,326,842 C2Siallite double component wet cement, method of production and use20082
US 6,394,707 B1Yieldable mine roof support200256
US 6,758,896 B2Rapid hardening, ultra-high early strength portland-type cement compositions, novel clinkers and methods for their manufacture which reduce harmful gaseous emissions200416
KR 100,466,947 B1Polymer mortar and method repair or supplementary concrete20054
JP 2006515260 Aシアライト2成分系湿式セメント、その製造方法および使用方法—10