US 5,093,290 A#28118318 Most CitedExpiredUnited States (USPTO)Utility

Silicon nitride type sintered bodies and method for producing the same

3Forward Citations (#28118318 Global)
0.1/yrCitation Velocity (#46643694 Global)
1.65Citation PageRank (#19755773 Global)
16Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

PCT No. PCT/JP89/00687 Sec. 371 Date Mar. 2, 1990 Sec. 102(e) Date Mar. 2, 1990 PCT Filed Jul. 7, 1989 PCT Pub. No. WO90/00531 PCT Pub. Date Jan. 25, 1990.The deterioration of strength at high temperature of Si3N4-Y2O3-AlN series silicon nitride-type sintered bodies is reduced by employing Y2O3-MgO-AlN series as a sintering aid wherein the stoichiometrical ratio of Y, Mg and Al in the sintered body is controlled to a specific range, thereby decreasing the glass phase to decrease deterioration of strength at high temperatures. Assuming Y as A1 mol, Mg as B1 mol and A1 as C1 mol based on one mol of Si3N4 in the sintered body, the specific range, wherein each of A1, B1 and C1 is not less than 0, satisifies the conditions: -0.03 </= C1 - (A1 + B1) </= 0.03 mol; 0.1 </= A1 + B1 + C1 </= 0.4 mol; and 0.2 </= B1/A1 </= 1.2 and the crystal phase of Si3N4 consisting of an alpha -Si3N4 phase in which a part of Si3N4 is replaced by Y, Mg, O and Al, and a beta -Si3N4 phase in which a part of Si3N4 is replaced by Al and O, and a balance of a binding glass phase comprising Si, Al, O, N, Y and MG, wherein the ratio between the alpha -Si3N4 phase and beta -Si3N4 phase is defined

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 3.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A silicon nitride-type sintered body produced from Si 3 N 4 , Y 2 O 3 , MgO and AlN powder, wherein Y, Mg and Al are present in amounts greater than 0 satisfying the following conditions: ##EQU7## said sintered body having a microstructure consisting of a crystalline phase of Si 3 N 4 and a glassy binder phase, said crystalline phase of Si 3 N 4 consisting of α-Si 3 N 4 partially-substituted with Y, Mg, O and Al and β-Si 3 N 4 partially-substituted with Al and O, said Al being substantially provided from said AlN powder, said glassy binder phase consisting of Si, Al, O, N, Y and Mg

  2. Claim 2Depends on #1

    A silicon nitride-type sintered body produced from Si 3 N 4 , Y 2 O 3 , Mgo and AlN powder as in claim 1 further having dispersed therein a Ti component selected

Technical Overview & Description