US 5,091,019 A#27508130 Most CitedExpiredUnited States (USPTO)Utility

Rapidly solidified aluminum lithium alloys having zirconium

3Forward Citations (#27508130 Global)
0.1/yrCitation Velocity (#46488714 Global)
2.90Citation PageRank (#7996556 Global)
5Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A rapidly solidified, low density aluminum base alloy consisting essentially of the formula Al ba1 Li a Cu b MG c Zr d wherein "a" ranges from about 2.1 to 3.4 wt %, "b" ranges from about 0.5 to 2.0 wt %, "c" ranges from about 0.2 to 2.0 wt % and "d" ranges from about 0.4 to 1.8 wt %, the balance being aluminum is consolidated to produce a strong, tough low density article.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 3.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A rapidly solidified, low density aluminum base alloy consisting essentially of the formula Al bal Li a Cu b Mg c Zr d wherein "a" ranges from about 2.1 to 3.4 wt %, "b" ranges from about 0.5 to 2.0 wt %, "c" ranges from about 0.2 to 2.0 wt % and "d" ranges from about 0.4 to 1.8 wt %, the balance being aluminum.

  2. Claim 2Depends on #1

    An alloy as recited in claim 1, wherein "a" ranges from about 2.8 to 3.0 wt %, "b" ranges from about 0.8 to 1.2 wt %, "c" ranges from about 0.4 to 0.6 wt %, and "d" ranges from about 0.7 to 1.6 wt %.

  3. Claim 3Depends on #2

    A consolidated article as recited in claim 2, having a 0.2% tensile yield strength of 470 MPa, ultimate tensile strength of 550 MPa, tensile elongation to fracture of 5%, and a V-notch impact energy of 5.0×10 -2 Joules/mm 2 .

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗