Abstract

Aromatic sulfide/ketone polymer is prepared from dihaloaromatic ketone, alkali metal sulfide, water and a polar organic compound. The polymerization reaction mixture comprising the aromatic sulfide/ketone polymer is subjected to a heat soak at elevated temperature then a separation agent (non-solvent) is added under controlled conditions and subsequently cooled to provide a mixture comprising particulate aromatic sulfide/ketone polymer. Biaxially-oriented film is made from recovered particles of aromatic sulfide/ketone polymer prepared as described by (1) washing the polymer particles with an aqueous calcium salt, (2) heating said washed particles to remove water, wherein the resulting heated particles are at least partially crystalline, (3) molding said heating particles to form a sheet of polymer, (4) biaxially stretching said sheet above the glass transition temperature of the polymer to form a film, and (5) heat-setting said biazially-oriented film under stretching tension for a time and at a temperature to increase strength properties and density.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 3.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for preparing aromatic sulfide/ketone polymer comprising the steps of a) charging to a polymerization reaction vessel, and thereby contacting at least one polar organic compound, at least one dihaloaromatic ketone, at least one alkali metal sulfide, and water under polymerization conditions effective for producing a first polymerization reaction mixture; b) heating said first polymerization reaction mixture to an elevated temperature of about 280° C. to about 350° C. and maintaining said first polymerization reaction mixture at said elevated temperature for about 10 seconds to about

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗