Pressed parts based on pyrogenically produced silicon dioxide, method of their production and their use
Abstract
Pressed parts based on pyrogenically produced silicon dioxide with the following physicochemical characteristic data: -Outer diameter 2 to 15 mm -BET surface 50 to 400 m2/g -Pore volume 0.6 to 1.3 ml/g -Breaking strength 50-150 N -Pore distribution no pores <5 mn diameter - only meso and macropores -Composition >99% by weight SiO2 -Abrasion <1.0% -Bulk weight: 400-500 g/l - are produced by homogenizing pyrogenically produced silicon dioxide with urea, methyl cellulose and/or magnesium stearate, graphite and aluminum stearate with the addition of water, dried at a temperature of 80 DEG to 120 DEG C., comminuted to a powder, pressing the powder to pressed parts and tempering the pressed parts for a period of 0.5 to 8 hours at a temperature of 400 DEG to 1200 DEG C.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 31.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
Shaped articles comprising phyrogenically produced silicon dioxide, said shaped articles having the following physicochemical characteristic data: ______________________________________ Outer diameter 2 to 15 mm BET surface 50 to 400 m.sup.2 /g Pore volume 0.6 to 1.3 ml/g Breaking 50-150 N strength Pore distribution no pores <5 [nm] diameter, only meso and macropores Composition >99% by weight SiO.sub.2
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗