Hydrazine bath for chemical deposition of platinum and/or palladium, and method of manufacturing such a bath
Abstract
The bath contains an oxalate of the metal or of each of the metals to be deposited and hydrazine as a reducing agent, together with ethylenediamine as a complexing agent and at least one stabilizing agent, said bath being highly basic and having an autocatalytic effect.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 19.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
An aqueous bath for chemical deposition of platinum and/or palladium, said bath comprising an oxalate compound of the metal or each of the metals to be deposited, hydrazine as a reducing agent, ethylenediamine as a complexing agent, and at least one stabilizing agent, wherein said bath contains essentially no chloride ions, is highly basic and has an autocatalytic effect.
- Claim 2Depends on #1
A bath according to claim 1, containing platinum II at a concentration lying in the range about 0.05 gram ions to about 0.15 gram ions.
- Claim 3Depends on #2
A bath according to claim 2, containing the following ingredients in the following molar ranges: ethylenediamine: 0.1 to 4 oxalate anions: 0.05 to 0.15 arsenic pentoxide: 10 -5 to 5×10 -3 imidazole: 0.2 to 0.5 hydrazine: 0.05 to 5 its pH lying in the range about 10 to about 14.
Technical Overview & Description