Preparation of foams having high heat-distortion resistance, and foams based on aromatic polyether ketones
Abstract
Foams of density 0.1 to 1.0 g/cm 3 based on aromatic polyether ketones and other thermoplastic polymers having a high melting point are obtained by melting an intimate mixture of the polymer and from 0.5 to 10% by weight of an aliphatic or aromatic dicarboxylic acid or polycarboxylic acid which suffers a weight loss of 50% or more with elimination of gaseous decomposition products on heating to from 130 to 300° C., and simultaneously cooling and molding the melt.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 3.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A process for the preparation of a foam having high heat-distortion resistance, which comprises melting an intimate mixture of (a) a thermoplastic polymer having a softening point (melting point) of above 200° C., selected from the group consisting of a polyamide, a polyester of an aromatic dicarboxylic acid, an aromatic polysulfone, a polyether sulfone and an aromatic polyether ketone, and (b) from 0.5 to 10% by weight, relative to (a), of an aliphatic or aromatic dicarboxylic acid or polycarboxylic acid which suffers a weight loss of 50% or more with elimination of gaseous decomposition pr
- Claim 2Depends on #1
A process as claimed in claim 1, wherein component b) used is an aliphatic dicarboxylic acid having from 2 to 8 carbon atoms, which may contain a hydroxyl