Patents
US 5,069,887 A#971067 Most CitedExpiredUnited States (USPTO)Utility

Method of refining nitrogen trifluoride gas

49Forward Citations (#971067 Global)
1.4/yrCitation Velocity (#3908543 Global)
6.94Citation PageRank (#1942421 Global)
8Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The invention provides a selective adsorption method for refining NF 3 gas containing CF 4 as impurity. At a temperature not higher than 10° C. the NF 3 gas is brought into contact with a crystalline and porous synthetic zeolite, which is substantially uniform in pore size and about 4.9 Å in effective pore size and is commerciallized under the name of molecular sieve 5A, on condition that the content of water of crystallinity in the synthetic zeolite is 1-10 wt. %, and preferably 6-10 wt. %. The synthetic zeolite efficiently adsorbs NF 3 with little adsorption of CF 4 .

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 49.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of refining a nitrogen trifluoride gas containing CF 4 as impurity, the method comprising the steps of: (a) bringing said nitrogen trifluoride gas into contact with a crystalline and porous synthetic zeolite, which is substantially uniform in pore size and about 4.9 Å in effective pore size, on condition that the content of water of crystallinity in said synthetic zeolite is in the range from 4 to 10 wt% and that said synthetic zeolite is maintained at a temperature not higher than 10° C. to thereby allow said synthetic zeolite to selectively adsorb NF 3 gas; (b) after step (a) sh

  2. Claim 2Depends on #1

    A method according to claim 1, wherein s

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗