US 5,069,867 A#5749827 Most CitedExpiredUnited States (USPTO)Utility

Process of manufacturing high-strength sintered members

16Forward Citations (#5749827 Global)
0.5/yrCitation Velocity (#17700080 Global)
3.01Citation PageRank (#7524650 Global)
4Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

To permit an economical manufacture of high-strength sintered members for use in valve timing mechanisms of internal combustion engine by powder metallurgy with liquid-phase sintering, an iron-base powder mixture is provided, which contains 13 to 18% by weight chromium or 3 to 6% by weight molybdenum as a carbide-forming alloying element in the iron alloy powder and also contains 1.5 to 2.6% carbon and 0.4 to 1.0% by weight phosphorus. A corresponding molten iron alloy is atomized into an entraining gas or water jet and is subsequently mixed with the remaining components of the powder.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 16.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    In a process of manufacturing a high-strength sintered member, comprising providing a carbon-containing powder mixture comprising an iron alloy powder, which contains at least one carbide-forming alloying element of group VIb of the periodic system, compacting said powder mixture to form a compact, and subjecting said compact to liquid-phase sintering, the improvement residing in that said powder mixture is provided to comprise an iron alloy powder containing at least one carbide-forming alloying element selected from the group consisting of chromium in an amount of 13 to 18% by weight,