Abstract
An expendable pattern of an article to be cast comprises a meltable material that expands upon heating (e.g., a wax pattern). The pattern is invested with particulate mold material to form a thin, layered shell having a wall thickness not exceeding about 0.12 inch. The thin shell wall thickness unexpectedly reduces damage and distortion to the shell during removal of the pattern therefrom by steam autoclaving. After firing, the thin gas permeable shell mold is surrounded by a refractory particulate support media in a vacuum housing. The vacuum housing is then evacuated to evacuate the mold cavity defined by the thin shell and concurrently a pressure is applied to the support media so as to compress the support media about the thin shell to support the shell against casting stresses when molten metal is countergravity cast into the evacuated mold cavity.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 73.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of countergravity casting molten metal, comprising the steps of: (a) forming an expendable pattern of an article to be cast, said pattern comprising a meltable material that expands upon heating, (b) investing the pattern with particulate refractory mold material in multiple layers so controlled as to form a thin, refractory shell having a wall thickness not exceeding about 0.12 inch, (c) heating the invested pattern to remove the pattern from the thin shell to leave a mold cavity therein, (d) disposing a refractory particulate support media about the thin shell with the mold ca
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗