Patents
US 5,068,084 A#2106137 Most CitedExpiredUnited States (USPTO)Utility

Columnar grain superalloy articles

31Forward Citations (#2106137 Global)
0.9/yrCitation Velocity (#8002178 Global)
9.19Citation PageRank (#1219446 Global)
15Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

An article exhibiting superior mechical properties and resistance to oxidation corrosion at elevated temperatures as described. The article has particular utility in gas turbine engines and is comprised of a nickel base superalloy consisting essentially of 3-10% Cr, 12.1-16% Co, 1.0-1.9% Mo, 3-10% W, 0-5% Re, 4-7% Al, 0-1.5% Ti, 0-8% Ta, 0.5-3% Hf, 0-2% Cb, 0-1% V, 0.02-0.12% Zr, 0.03-0.2% C, 0.005-0.25% B, 0-0.15% of an oxygen active element such as yttrium, balance essentially nickel. This composition is melted and directionally solidified in columnar grain form to provide useful articles.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 31.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A superalloy composition suited for the fabrication of columnar grain articles which consists essentially of: 3-10% Cr 2.1-16.0% Co 1.0-1.9% Mo 3-10% W 0-5% Re 4-7% Al 0-1.5% Ti 0-8% Ta 0.5-3.0% Hf 0-2% Cb 0-1% V 0.02-0.12% Zr 0.03-0.20% C 0.005-0.25% B 0-10% reactive element Balance Ni.

  2. Claim 2Depends on #1

    A composition as in claim 1 having incipient melting temperature sufficiently high to permit heat treatment, said composition satisfying the relationship 70+5 Cr+3 Co-(25 Ti+7 Ta+15 Al)≧O.

  3. Claim 3Depends on #1

    A composition as in claim 1 having good hot corrosion resistance, and in which the following relationship is satisfied: 2 Cr-2(Mo+W)≧O.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗