Making pressed board
Abstract
A fiber or chip board is made by first forming a mixture of a binder and particles having a relatively low moisture content that is substantially less than a relatively high moisture content that a finished board should have. This mixture is deposited as a mat on a movable substrate so that the mat is substantially at ambient temperature and has the relatively low moisture content. Then the mat is preheated with steam to raise its temperature and to increase its moisture content to the predetermined relatively high moisture content. The thus preheated mat, whose moisture content has been corrected, is then simultaneously heated and compressed to form it into a board.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 41.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
A method of making a board, the method comprising the steps of sequentially: forming a mixture of an aqueous binder and particles having a relatively low moisture content of between 5% and 10% by weight; depositing the mixture as a mat on a movable substrate, the mat being substantially at ambient temperature and having the relatively low moisture content; preheating the mat with steam at a temperature of between 100° C. and 140° C. to raise the mat's temperature and to increase its moisture content to a relatively high moisture contents of between 10% and 15% by weight; and simultan
- Claim 2Depends on #1
The board-making method defined in claim 1, further comprising the step of: mixing the particles with a binder prior to deposition onto the substrate.
- Claim 3Independent Claim
The bo
Technical Overview & Description