Patents
US 5,049,221 A#565753 Most CitedExpiredUnited States (USPTO)Utility

Process for producing a copper-clad laminate

65Forward Citations (#565753 Global)
1.9/yrCitation Velocity (#2370280 Global)
10.41Citation PageRank (#992397 Global)
5Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A process for producing a copper-clad laminate, which comprises a step (S2) of forming a copper foil of at least several micrometers on a planar conductive substrate by electrolysis, a step (S3) of roughening the surface of the copper foil, a step (S4) of laminating the copper foil together with the conductive substrate on an insulating substrate and tightly integrating the assembly by applying pressure and heat, and a step (S5) of separating only the conductive substrate. A metal film may exist between the conductive substrate and the copper foil. When the metal film has a thickness of 0.1 to 3 μm, only the conductive substrate is separated with the metal film being firmly adhered to the copper foil surface and, when the metal film has a thickness of 70 to 250 μm, it is separated together with the conductive substrate after the lamination. The copper foil formed by high-speed plating under the conditions of 6 to 12.0 m/sec in solution contact speed and 0.8 to 4.0 A/cm 2 in current density has about the same flexibility as that of rolled and annealed copper. Thus, ultrathin copper-clad laminates with a copper foil of 10 μm or less suited for flexible circuit boards can be produced

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 65.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for producing a copper-clad laminate, comprising the steps of: providing a planar cathode comprising an electrically conductive substrate and a metal film 70 to 250 μm thick plated onto a surface of said electrically conductive substrate; said metal film being a two-component alloy layer consisting essentially of 60% to 80% by weight of nickel and 20% to 40% by weight of cobalt; forming a copper foil having a thickness of not more than 10 μm directly on the surface of said metal film at a deposition speed of 25 to 100 μm/min, by electroplating under the conditions that said planar

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 65 total)

PatentTitleYearCitations
US 2006076422 A1Conductive pattern and method of making—6
US 10,464,291 B2Copper heat dissipation material, carrier-attached copper foil, connector, terminal, laminate, shield material, printed-wiring board, metal processed member, electronic device and method for manufacturing the printed wiring board20191
US 7,829,180 B2Composition for forming adhesive pattern, laminated structure obtained by using same, and method of producing such laminated structure20106
US 5,362,926 ACircuit substrate for mounting a semiconductor element199442
US 6,431,750 B1Flexible temperature sensing probe200232
US 7,930,815 B2Conductive pattern and method of making201115
US 5,403,465 AElectrodeposited copper foil and process for making same using electrolyte solutions having controlled additions of chloride ions and organic additives199530
US 7,731,831 B2Method for manufacturing a composite material including copper foil and support layer20103
US 6,985,348 B2Laminated electronic part20063
US 5,779,870 AMethod of manufacturing laminates and printed circuit boards199831
US 5,792,375 AMethod for bonding copper-containing surfaces together199815
US 2006057819 A1Electronic part producing method and electronic part—0
US 2002041032 A1Copper clad laminate—7
US 2004144656 A1Plating bath for forming thin resistance layer, method of formation of resistance layer, conductive base with resistance layer, and circuit board material with resistance layer—11
US 5,454,926 AElectrodeposited copper foil199519