Method for producing high opacifying kaolin pigment
Abstract
A method of producing a high opacity paper filler pigment which comprises subjecting an iron-stained titania-containing kaolin to beneficiation by froth flotation or high intensity magnetic separation; recovering the froth or magnet rejects, dewatering and drying the rejects to produce a kaolin enriched in titania, and calcining the same at a temperature in the range of about 1500° to about 2200° F.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 22.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of producing a high opacifying pigment which comprises subjecting an iron-stained titania-containing kaolin to froth flotation, recovering froth "rejects" comprising kaolin enriched in said iron-stained titania, said enriched kaolin containing said titania in the amount of above 2weight percent to about 15 weight percent, dewatering and drying said froth "rejects", and calcining said "rejects" having above 2 to about 15 weight % titania at a temperature in the range of about 1500° to about 2200° F.
- Claim 2Depends on #1
The method according to claim 1 in which the froth "rejects" are not further beneficiated prior to calcining.
- Claim 3Depends on #1
The method according to claim 1 in which the starting material is a naturally occurring kaolin having a titania content of from about 1 to 2 weight %. 4
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗