Patents
US 5,047,367 A#123129 Most CitedExpiredUnited States (USPTO)Utility

Process for formation of a self aligned titanium nitride/cobalt silicide bilayer

136Forward Citations (#123129 Global)
3.9/yrCitation Velocity (#500791 Global)
47.08Citation PageRank (#79000 Global)
6Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A process for the formation of a titanium nitride/cobalt silicide bilayer for use in semiconductor processing. Titanium and then cobalt are deposited on a silicon substrate by sputter deposition techniques. The substrate is then annealed. During this process the titanium first cleans the silicon surface of the substrate of any native oxide. During the anneal, the titanium diffuses upward and the cobalt diffuses downward. The cobalt forms a high quality epitaxial cobalt silicide layer on the silicon substrate. The titanium layer diffuses upward to the surface of the bilayer. The anneal is carried out in a nitrogen or ammonia ambient, so that a titaniun nitride layer is formed. The resulting structure can be used in self aligned silicide technology, as a contact fill material for contact to electrical regions of the device, and as a diffusion barrier preventing the diffusion of aluminum from a subsequently deposited aluminum layer or the diffusion of dopants from a subsequently grown doped selective silicon layer into the silicon substrate.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 136.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A process for forming a bilayer on a silicon substrate comprising the steps of: conformally depositing on said silicon substrate a first layer comprising a refractory metal; conformally depositing on said first layer a second layer comprising a near-noble metal; performing an anneal on said silicon substrate in a nitrogen containing gas selected from the group consisting of nitrogen and ammonia to form a near-noble metal silicide layer disposed above said silicon substrate and a refractory metal nitride layer disposed above said near-noble metal silicide layer.

  2. Claim 2Depends on #1

    The process as described in claim 1 wherein said near-noble metal silicide layer has a thickness in the range of 300-2000 Angstroms and said refractory metal nitride layer has a thickness in the range of 50-500 Angstroms.

  3. Claim 3Independent Claim

    The process as described in cla

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (3)

  • Cobalt Silicide Interconnection from a Si/Uv/Lo Trilayer Structure; Lin et al.; J. Electrochem. Soc. vol. 136, No. 1; 1/89.
  • Novel Submicron MOS Devices by Self Aligned Nitridation of Silicide; Kaneko et al.; 1985 IEEE; pp. 208 211.
  • Novel Submicron MOS Devices by Self-Aligned Nitridation of Silicide; Kaneko et al.; 1985 IEEE; pp. 208-211.