Abstract
There is described an improved bipolar electrode comprised of an intermediate double-sided adhesive conductive plastic film or layer disposed between electronegative and electropositive layers wherein the intermediate layer has a volume resistivity of at least 0.5 ohm-cm. as well as a process for manufacturing same by passing a laminate of such layers through a pressure roller assembly at pressures between 30 to 500 psig.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 1 · Forward citations: 2.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A process for forming a bipolar electrode structure which comprises: a) introducing into a nip of a pressure roller assembly a laminate comprised of an electronegative layer; an electrically conductive impermeable intermediate layer of a thickness of 0.5 to 5 mils, a volume resistivity of 0.5 to 100 ohm-cm. and having pressure sensitive adhesive surfaces and an electropositive layer; b) passing said laminate through said pressure roller assembly at a pressure of from 20 to 500 psig. to effect adhesion of said electronegative and electropositive layers; and c) withdrawing said bipolar elect
- Claim 2Depends on #1
The process for forming a bipolar electrode structure as defined in claim 1 wherein said pressure roller assembly is heated to a temperature of from 30° to 180° F.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
References Cited — Backward Prior Art (1)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 4,502,903 A | Method of making lithium batteries with laminar anodes | 1985 | 60 |