Patents
US 5,035,781 A#17064830 Most CitedExpiredUnited States (USPTO)Utility

Electrolyte for the production of black surface layers on light metals

6Forward Citations (#17064830 Global)
0.2/yrCitation Velocity (#36021538 Global)
1.88Citation PageRank (#16000525 Global)
5Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The invention relates to a cyanide-free electrolyte being harmless to the environment and to health which makes feasible the production of black surface layers on light metals or on alloys of the latter, preferably titanium, remaining deeply-black and adhesive even after extreme changes in the ambient temperature and having nearly equal values of the optical absorptivity of radiation and of the thermal emission capability (the α/ε-ratio is about 0.95) by means of the anodic oxidation by spark discharge (ANOF-method). These layers are absolutely X-amorphous and show, hence, an ideal optically isotropic behavior regarding the reflection of radiation. Due to their minimum evolution of gases they offer a high thermovacuum stability. The electrolyte consists of an ammoniacal solution of K 2 H 2 PO 4 potssium dihydrogenphosphate and K 2 CRO 4 potassium chromate. The homogeneity of the optically black layers is ensured by not using fluoride ions and employing acetate ions. Such layers comprise titanium, chromium and copper following ratios of CR:Ti=1:(1.9 to 2.2) and CR:Cu=1:(0.8 to 1.3).

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 6.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    An electrolyte for the production of black surface layers on light metals or alloys thereof, preferably titanium, by means of an anodic oxidation by spark discharge, wherein the electrolyte consists of a 2 to 6 percent by volume ammoniacal acqueous solution of 0.3 to 0.6 mole/liter potassium dihydrogenphosphate; 0.08 to 0.3 mole/liter potassium chromate and of acetate ions in concentrations of 0.08 to 0.5 mole/liter.

  2. Claim 2Depends on #1

    The electrolyte of claim 1, wherein the acetate ions of copper acetate are employed.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗