Heat treating method for high strength aluminum alloy
Abstract
A heat treating method for a high strength aluminum alloy comprising the steps of: solution heat treating of an aluminum alloy consisting essentially of about 3 to 9 wt. % Zn, 1 to 6 wt. % Mg, 1 to 3 wt. % Cu, at least one element selected from the group consisting of 0.1 to 0.5 wt. % Cr, 0.1 to 0.5 wt. % Zr, 0.2 to 1.0 wt. % Mn, and the balance being Al, heating of the solution heat treated alloy to a temperature of a lower temperature zone of from 100° to 140° C. and optionally maintaining the alloy at a temperature within the lower temperature zone for a duration of time, reheating of the alloy to a temperature of an upper temperature zone of from 160° to 200° C. and optionally maintaining the alloy at a temperature within the upper temperature zone for a second duration of time, cooling of the alloy to a temperature of the lower temperature zone, and repeating the steps (2), (3), and (4) at least twice.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 15.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A heat treating method for high strength aluminium alloy comprising the steps of; (1) solution heat treating an aluminium alloy consisting essentialy of about 3 to 9 wt. % Zn, 1 to 6 wt. % Mg, 1 to 3 wt. % Cu, at least one element selected from the group consisting of 0.1 to 0.5 wt.% Cr, 0.1 to 0.5 wt.% Zr, 0.2 to 1.0 wt.% Mn, and the balance Al, (2) heating the solution heat treated alloy to a temperature of a lower temperature zone of from 100° to 140° C. and optionally maintaining said alloy at a temperature within said lower temperature zone for a duration of time, (3) reheating of the
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗