Tree resistant compositions
Abstract
1. A composition comprising: (a) a homopolymer of ethylene having a density in the range of about 0.915 to about 0.925 gram per cubic centimeter and a melt index in the range of 0.1 to about 5 grams per 10 minutes or a copolymer of ethylene and one or more alpha-olefins, each having 3 to 8 carbon atoms, said copolymer having a density in the range of about 0.880 to about 0.915 grams per cubic centimeter and a melt index in the range of about 0.1 to about 10 grams per 10 minutes; and p1 (b) a polysiloxane having the formula: ##STR1## wherein: R=alkyl having 1 to 4 carbon atoms, acyl having 1 to 4 carbon atoms, or trimethyl silyl, and each R is alike or different R'=alkyleneoxy having 3 to 11 carbon atoms R"=hydrogen or alkylhydroxy having 3 carbon atoms and 2 hydroxyl groups. x=about 2 to about 20 y=about 2 to about 20, and the hydroxyl content of the composition is at least about 0.15 percent by weight based on the total weight of the composition.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 21.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A composition comprising: (a) a homopolymer of ethylene having a density in the range of about 0.915 to about 0.925 gram per cubic centimeter and a melt index in the range of 0.1 to about 5 grams per 10 minutes or a copolymer of ethylene and one or more alpha-olefins, each having 3 to 8 carbon atoms, said copolymer having a density in the range of about 0.880 to about 0.915 gram per cubic centimeter and a melt index in the range of about 0.1 to about 10 grams per 10 minutes; and (b) a polysiloxane having the formula: ##STR4## wherein: R=alkyl having 1 to 4 carbon atoms, acyl having 1 to 4 ca
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗