Method for depositing highly erosive and abrasive wear resistant composite coating system on a substrate
Abstract
The method for producing the disclosed material comprises chemical vapor depositing on the substrate a substantially columnar, intermediate layer of tungsten and chemical vapor depositing on the intermediate layer a non-columnar, substantially lamellar outer layer of a mixture of tungsten and tungsten carbide. The tungsten carbide comprises W 2 C, W 3 C, or a mixture of both wherein the ratio of the thickness of the tungsten intermediate layer to the thickness of the outer layer is at least: (a) 0.35 in the case of tungsten plus W 2 C in the outer layer, (b) 0.6 in the case of a mixture of tungsten and W 3 C in the outer layer and (c) 0.35 in the case of mixtures of tungsten and W 2 C and W 3 C in the outer layer. The chemical vapor deposition steps are carried out at pressures within the range of 1 Torr to 1,000 Torr and temperatures within the range of about 300° to about 650° C.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 19.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for producing a highly erosion and abrasion wear resistant composite coating system on a substrate selected from the group consisting of ferrous metals and alloys, non-ferrous metals and alloys, graphite, carbides and ceramics, comprising, chemical vapor depositing on the substrate a substantially columnar, intermediate layer of tungsten of sufficient thickness to confer substantial wear resistant characteristics on said coating system using a gaseous mixture of tungsten halide and hydrogen at pressures within the range of about 1 Torr. to about 1,000 Torr and a temperature of about 3
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗