Long-laser-pulse method of producing thin films
Abstract
A method of depositing thin films by means of laser vaporization employs a long-pulse laser (Nd-glass of about one millisecond duration) with a peak power density typically in the range 10 5 -10 6 W/cm 2 . The method may be used to produce high T c superconducting films of perovskite material. In one embodiment, a few hundred nanometers thick film of YBa 2 Cu 3 O 7-x is produced on a SrTiO 3 crystal substrate in one or two pulses. In situ-recrystallization and post-annealing, both at elevated temperature and in the presence of an oxidizing agen The invention described herein arose in the course of, or under, Contract No. DE-C03-76SF0098 between the United States Department of Energy and the University of California.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 26.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method of depositing a thin film of a superconducting ceramic material on a substrate by laser evaporation, comprising the steps of: providing a solid target of the material and the substrate spaced therefrom in an evacuated chamber; maintaining the substrate at a first predetermined elevated temperature; vaporizing a portion of the material from the target by a laser beam having a peak power density in the range between 10 5 -10 6 W/cm 2 and a pulse width in the range between 0.5 to 2.0 milliseconds; and forming the a thin film of the superconducting ceramic material on the substra
- Claim 2Depends on #1
The method as in claim 1, further comprising: providing a predetermined metered amount of reactive oxidation agent adjacent to the surface of the substrate to be coated, the oxidizing agent being add
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 26 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.
Non-Patent Literature (5)
- "High Tc Superconducting Thin Films . . . ", Lynds et al., Amer. Inst. of Phys., 159-160 (Nov. 6, 1987).
- "Highly Oriented As-Deposited Superconducting Laser . . . ", Appl. Phys., 53(23):2330-2332 (Dec. 5, 1988).
- "Laser Evaporation Deposition of Superconducting . . . ", Kwok et al., Appl. Phys., 52(21):1825-1827 (Mar. 30, 1988).
- "Laser Induced Deposition . . . ", Kwok et al., Mat. Res. Soc. Symp., 99:273-277 (1988).
- "Laser Induced Deposition of . . . ", Kwok et al., Mat. Res. Soc. Symp. Proc., 99:735-737 (1988).