Alloy for building JP valve
Abstract
An alloy for building up a valve according to the present invention comprises: with respect to the total weight of the alloy taken as 100%, 30 to 40% by weight of chromium; 15 to 31% by weight of nickel; 7 to 20% by weight of molybdenum; 0.7 to 2.2% by weight of carbon; 1.5% or less by weight of silicon; and balance of iron and inevitable impurities. The alloy is superior in hardness at high temperatures, PbO resistance and PbO+PbSO 4 resistance. In addition, the alloy is suitable for powder buildup welding.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 3.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
An alloy for building up a valve consisting essentially of, with respect to the total weight of said alloy taken as 100%, 30 to 40% by weight of chromium; 15 to 31% by weight of nickel; 7 to 20% by weight of molybdenum; 0.7 to 2.2% by weight of carbon; 1.5% or less by weight of silicon; and balance of iron and inevitable impurities, and said alloy being in a form of powder having a size in the range of 80 to 350 mesh.
- Claim 2Depends on #1
An alloy for building up a valve according to claim 1, wherein the content of said chromium is 33 to 38% by weight.
- Claim 3Depends on #1
An alloy for building up a valve according to claim 1, wherein the content of said nickel is 17.0 to 27.5% by weight.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗