Patents
US 5,017,346 A#22872699 Most CitedExpiredUnited States (USPTO)Utility

Process for treating zinc oxide bearing materials

4Forward Citations (#22872699 Global)
0.1/yrCitation Velocity (#43495461 Global)
2.13Citation PageRank (#13110111 Global)
16Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A process of refining zinc oxide from roasted zinc sulphide bearing concentrates comprises leaching the concentrate in an aqueous sulphur dioxide solution under controlled conditions providing selective separation of zinc from other elements contained in the concentrate. The zinc bisulphite solution so obtained is separated from the remaining solids and is heat treated, preferably with steam, to precipitate zinc monosulphite crystals, possibly after first adding zinc dust to the solution to cement out residual copper and cadmium. The zinc monosulphite is then separated from the solution, possibly washed with water, and calcined to yield purified zinc oxide.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 4.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for the refining of zinc oxide bearing material comprising the steps of: (a) leaching the zinc oxide bearing material by slurrying it in an aqueous sulphur dioxide solution, maintaining the slurry at a feed pulp density of about 100 to about 350 grams per liter, a temperature of about 0° C. to about 25° C., a pH value from about 2.0 to about 3.5, and the leaching residence time is adjusted to obtain maximum extraction of zinc consistent with minimum extraction of impurities; (b) subjecting the leach slurry of step (a) to liquid-solid separation to yield a zinc bearing leachate and

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗