Patents
US 5,000,797 A#26885812 Most CitedExpiredUnited States (USPTO)Utility

Method for producing a stainless steel having a good corrosion resistance and a good resistance to corrosion in seawater

4Forward Citations (#26885812 Global)
0.1/yrCitation Velocity (#43894303 Global)
1.14Citation PageRank (#34493883 Global)
3Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A stainless steel fundamentally comprises of, by weight, not more than 0.03% C., not more than 2.0% Si, not more than 5.0% Mn, 6-13% Ni, 16-21% Cr, 0.10-0.30% of N, and 0.02-0.25% Nb with the balance being Fe and inevitable impurity elements. The steel has a good corrosion resistance and a resistance to corrosion in seawater. The steel may further comprise at least one member of Mo and Cu each in an amount of not more than 0.4% S, Se and Te each in an amount of not more than 0.08% Bi, Pb, V, Ti, W, Ta, Hf, Zr and Al each in an amount of not more than 0.30% and P, Ca, Mg and rare earth elements each in an amount of not more than 0.01%. The steel has a recrystallized and worked double structure when subjected to a process comprising rough rolling an steel ingot at a temperature ranging from 1000 to 1200% at a working rate of not less than 50%, cooling at a cooling rate of not less than 4° C./min, subsequently finish rolling at a temperature ranging from 800° to 1000° C., at a working rate of not less than 20%, and cooling at a cooling rate of not less than 4° C./min.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 4.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of producing a stainless steel having a good corrosion resistance and a good resistance to corrosion in seawater comprising the steps of preparing a steel ingot from a steel including, by weight, not more than 0.03% C, not more than 2.0% Si, not more than 5.0% Mn, 6-13% Ni, 16-21% Cr, 0.10-0.30% N and 0.02-0.25% Nb, the remainder being Fe and inevitable impurities; heating said ingot to a temperature ranging from 1,100° to 1,300° C.; roughly rolling said ingot at a temperature ranging from 1,000° to 1,200° C. at a reduction rate of more than 50% and cooling rolled ingot under a coolin

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗