Anisotropic high energy magnets and a process of preparing the same
Abstract
A process of making anisotropic permanent magnets by extruding a rare earth magnetic alloy below the melting temperature of the alloy at an extrusion ratio of from 10:1 to 26:1.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 10.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A process of making anisotropic permanent magnets which comprises extruding a rare earth transition metal magnetic alloy at a temperature of from about 600° C. to about 1000° C. at an extrusion ratio of from about 10:1 to about 26:1.
- Claim 2Depends on #1
The process of claim 1 wherein the rare earth magnetic alloy is an alloy of neodymium, iron and boron.
- Claim 3Depends on #2
The process of claim 2 wherein the main magnetic phase in the magnetic alloy is Nd 2 Fe 14 B.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (10 of 10 total)
References Cited — Backward Prior Art (15)
Non-Patent Literature (4)
- "NdFeB Magnets Having a (100) Fiber Texture", B. M. Ma, R. F. Krause and V. Chandhok, Proceedings of the 9th International Workshop on Rare Earth Magnets and Their Application, Bad Soden, FRG, Aug. 31-Sep. 2, 1987--pp. 545-551.
- "Radially Oriented NdFeB Magnets", Bao-Min Ma, V. K. Chandhok, and E. J. Dulis--1987 Digest of Intermag Conference, Tokyo, Japan, Apr. 14-17, 1987.
- NdFeB Magnets Having a (100) Fiber Texture , B. M. Ma, R. F. Krause and V. Chandhok, Proceedings of the 9th International Workshop on Rare Earth Magnets and Their Application, Bad Soden, FRG, Aug. 31 Sep. 2, 1987 pp. 545 551.
- Radially Oriented NdFeB Magnets , Bao Min Ma, V. K. Chandhok, and E. J. Dulis 1987 Digest of Intermag Conference, Tokyo, Japan, Apr. 14 17, 1987.