Patents
US 5,000,791 A#5106295 Most CitedExpiredUnited States (USPTO)Utility

Process for the preparation of an acid-resistant coating on filler particles

17Forward Citations (#5106295 Global)
0.5/yrCitation Velocity (#17312272 Global)
6.77Citation PageRank (#2020639 Global)
7Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The invention relates to a process for the preparation of an acid-resistant coating and calcium carbonate particles, in which process a slurry of calcium carbonate particles is mixed simultaneously with the solution of a zinc compound and a solution of a silica-containing substance at a temperature of 70°-95° C., the pH being maintained at 8-11. The invention also relates to calcium carbonate particles having an acid-resistant coating in accordance with the above-mentioned process. In addition, the invention relates to the use of calcium carbonate particles having a acid-resistant coating in accordance with the above-mentioned process, as an acid-resistant filler in the production of paper at pH 4.0-7.0.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 17.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A process for the preparation of an acid-resistant coating on calcium carbonate particles, wherein a slurry of calcium carbonate particles is mixed simultaneously with a solution of a zinc compound and a solution of a silica-containing substance at a temperature of 70°-95° C., the pH being maintained at 8-11.

  2. Claim 2Depends on #1

    A process as claimed in claim 1, wherein the silica-containing compound is sodium water glass.

  3. Claim 3Depends on #1

    A process as claimed in claim 1, wherein the zinc compound is zinc chloride or zinc oxide.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 17 total)

PatentTitleYearCitations
EP 0,871,680 A4Surface modified calcium carbonate composition and uses therefor—0
US 5,527,430 AModified filler material for alkaline paper and method of use thereof in alkaline paper making199641
US 6,083,317 AStabilized calcium carbonate composition using sodium silicate and one or more weak acids or alum and uses therefor200030
WO 9,708,248 A1Surface modified calcium carbonate composition and uses therefor—3
US 5,599,388 AAcid resistant calcium carbonate composition containing an aluminum salt, uses therefor and processes for its production199714
WO 9,708,249 A1Acid resistant calcium carbonate composition containing an aluminum salt and uses therefor—3
EP 3,498,782 B1Preparation of silica-coated calcium carbonates with increased surface area and mesoporosity and silica hollow shells obtained from them20200
AU 701,251 B2Surface modified calcium carbonate composition and uses therefor19990
WO 0,026,305 A1Silica-coated alkaline earth metal carbonate pigment—4
US 6,623,555 B1Composite precipitated calcium carbonate/silicon compound pigment and method of making same200339
EP 0,848,736 A4Acid resistant calcium carbonate composition containing an aluminum salt and uses therefor—0
US 5,380,361 AModified filler material for alkaline paper and method of use thereof in alkaline paper making199518
CN 100,335,567 Ccalcium carbonate/silicon dioxide-water(1/n) nano-compound particle and hollow silicon dioxide-water(1/n) nano-material and its preparation method20070
US 5,584,923 ASurface modified calcium carbonate composition and uses therefor199630
US 5,164,006 AMethod for preparing acid resistant calcium carbonate pigments199244

Non-Patent Literature (2)

  • Patent Abstracts of Japan, vol. 10, No. 287 (JP A 61106673).
  • Patent Abstracts of Japan, vol. 10, No. 287 (JP-A-61106673).