Patents
US 4,990,179 A#34243222 Most CitedExpiredUnited States (USPTO)Utility

Process for increasing the life of carbon crucibles in plasma furnaces

2Forward Citations (#34243222 Global)
0.1/yrCitation Velocity (#51386508 Global)
2.78Citation PageRank (#8581169 Global)
9Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The excessive wear and formation of ring-like cavities in carbon crucibles used to contain iron-based compositions that are heated in a plasma furnace to a temperature of from about 2000° C. to aboout 2700° C. are reduced or eliminated by adding carbon particles to the crucible in amounts of at least about 6 weight percent of the melt, and preferably in amounts exceeding the solubility of carbon in the heated melt.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 2.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A process for reducing cavity formation in carbon crucibles used to contain iron-based compositions containing valuable metals in essentially a nonoxidized form that are heated in a plasma furnace to a temperature of from about 2000° C. to about 2700° C. to form a melt, comprising adding carbon particles to the crucible in amounts of at least about 6 weight percent of the melt but always in amounts at least equal to the solubility of carbon in the melt.

  2. Claim 2Depends on #1

    Process of claim 1 wherein the carbon particles are added in amounts exceeding the solubility of carbon in the melt at the melt temperature.

  3. Claim 3Depends on #1

    Process of claim 1 wherein the carbon particles are added in amounts of from about 6% to about 10 weight percent of the melt.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗