Patents
US 4,983,264 A#5094173 Most CitedExpiredUnited States (USPTO)Utility

Four layer cation exchange fluoropolymer membrane

17Forward Citations (#5094173 Global)
0.5/yrCitation Velocity (#17310391 Global)
8.37Citation PageRank (#1424770 Global)
10Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A cation exchange fluoropolymer membrane comprising at least three integrally laminated layers including a main layer made of a perfluorocarbon polymer having carboxylic acid groups as its ion exchange groups with an ion exchange capacity of from 1.4 to 2.0 meq/g dry resin and having a thickness of from 50 to 250 μm, a sulfonic acid film surface layer formed on one side of said main layer, made of a perfluorocarbon polymer having sulfonic acid groups as its ion exchange groups with an ion exchange capacity of from 0.5 to 1.5 meq/g dry resin and having a thickness of from 5 to 50 m, and a carboxylic acid film surface layer formed on the other side of said main layer, made of a perfluorcarbon polymer having carboxylic acid groups as its ion exchange groups with an ion exchange capacity of from 0.5 to 1.3 meq/g dry resin and having a thickness of from 5 to 50 μm, said sulfonic acid film surface layer and carboxylic acid film surface layer constituting the outer-most layers, respectively.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 17.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A cation exchange fluoropolymer membrane of high mechanical strength, having integrally laminated layers, consisting essentially of: (a) a main layer made of a perfluorocarbon polymer having carboxylic acid groups as ion exchange groups therefor with an ion exchange capacity of from 1.4 to 2.0 meq/g dry resin and having a thickness of from 50 to 250 μm; (b) a sulfonic acid film surface layer formed on one side of said main layer, made of a perfluorocarbon polymer having sulfonic acid groups as ion exchange groups therefor with an ion exchange capacity of from 0.5 to 1.5 meq/g dry resin and h

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (4)

  • Patents Abstracts of Japan, vol. 6, No. 239 (C 137) (1117), 26th Nov. 82; & JP A 57 141 428 (Toyo Soda Kogyo K.K.).
  • Patents Abstracts of Japan, vol. 6, No. 239 (C-137) (1117), 26th Nov. '82; & JP-A-57 141 428 (Toyo Soda Kogyo K.K.).
  • Patents Abstracts of Japan, vol. 6, No. 244 (C 138) (1122), 2nd Dec. 82; & JP A 57 143 332 (Toyo Soda Kogyo K. K.) 04 09 1982 *whole document*.
  • Patents Abstracts of Japan, vol. 6, No. 244 (C-138) (1122), 2nd Dec. '82; & JP-A-57 143 332 (Toyo Soda Kogyo K. K.) 04-09-1982 *whole document*.