Abstract

A process for increasing the content of mesophase in a pitch includes using a high molecular aromatic fraction based on a material selected from the group consisting of coal tar, crude oil and their mixture in molten form, thermally treating the fraction in form of a thin, continously moving film, and removing volatile components by degassing during the thermal treatment. The process distinguishes in using a high molecular aromatic fraction which may contain mesophase, shaping the fraction continuously mechanically to a thin film with a layer of thickness of between substantially 0.007 and 2 cm, successively mechanically forcedly transporting the film with the use of shear forces through at least one homogenization zone and one degassing zone, performing a mechanical homogenization of the film in the homogenization zone, performing a removal of readily volatile components in the degassing zone, and maintaining the temperature of the film in the homogenization zone and in the degassing zone in the region of between 320° C. and 470° C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 21 · Forward citations: 8.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for increasing the content of mesophase in a pitch, comprising the steps of using a high molecular aromatic fraction based on a material selected from the group consisting of coal tar, crude oil and their mixture in molten form, which aromatic fraction may contain mesophase, thermally treating said aromatic fraction, shaping the fraction continuously mechanically to form a thin film with a layer thickness of between substantially 0.007 and 2 cm, successively mechanically forcedly transporting the film with the use of shear forces to provide a thorough continuous mixing through at lea

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (21)

PatentTitleYearCitations
US 1,404,435 AProcess of presenting the hydrocarbon in the form of a thin film of large surface area to the action of an oxidizing agent19226
US 1,742,933 AProcess of mineral-oil distillation19304
US 1,794,542 ADistilling hydrocarbons19315
US 2,076,498 AFilm-forming means in vacuum system for removing impurities from oils193711
US 2,095,470 AMethod and apparatus for purifying liquids193710
US 2,732,332 AGeller19569
US 3,974,264 AProcess for producing carbon fibers from mesophase pitch197658
US 4,016,247 AProduction of carbon shaped articles having high anisotropy197730
US 4,042,486 AProcess for the conversion of pitch into crystalloidal pitch197732
US 4,243,512 AProcess for preparation of pitch for producing carbon fiber198126
US 4,259,171 AProcess for the separation of quinoline-insoluble components from coal tar pitch198127
US 4,271,006 AProcess for production of carbon artifact precursor198150
US 4,379,133 AProcess for anisotropic carbon production19835
GB 2,124,246 AProcess for preparing precursor pitch for carbon fibers—3
US 4,469,667 AProcess for production of pitch-derived carbon fibers198410
US 4,470,960 AProcess for the production of pitch-derived carbon fibers198415
US 4,497,789 AProcess for the manufacture of carbon fibers198531
US 4,551,225 AHigh anisotropic pitch198513
US 4,575,411 AProcess for preparing precursor pitch for carbon fibers19868
US 4,608,150 APitch material for carbonaceous body and a method for the preparation thereof19865
US 4,801,372 AOptically anisotropic pitch198914