Process for preparing thermally stable crosslinked epoxy resins
Abstract
Thermally stable, crosslinked epoxy resins are obtained by crosslinking an epoxy resin with a silicon compound containing a basic nitrogen which is bonded to silicon via carbon and to which at least 1 hydrogen atom is bonded directly to the nitrogen atom, and thereafter conditioning the crosslinked epoxy resin.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 9.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A process for preparing thermally stable, crosslinked epoxy resins which comprises crosslinking an epoxy resin with a silicon compound having a basic nitrogen which is bonded to silicon via carbon and to which at least 1 hydrogen atom is bonded directly to the nitrogen atom and thereafter conditioning the crosslinked epoxy resin at a temperature of from 150° C. to 250° C. for at least 2 hours.
- Claim 2Depends on #1
The process of claim 1, wherein at least part of the epoxy resin to be crosslinked comprises a product obtained from the reaction of 2,2-bis-(4-hydroxyphenyl)-propane and epichlorohydrin.
- Claim 3Depends on #1
The process of claim 1, wherein the silicon compound is an organopolysiloxane having units of the formula ##STR6## in which R is a monovalent hydrocarbon radical having from 1 to 8 carbon atoms per radical, R 1 is an alkyl group ha
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (9 of 9 total)
References Cited — Backward Prior Art (2)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 4,287,326 A | Siloxane-modified epoxy resin compositions | 1981 | 37 |
| US 4,413,104 A | Process for preparing organopolysiloxanes and copolymers thereof | 1983 | 23 |