Patents
US 4,968,356 A#12642265 Most CitedExpiredUnited States (USPTO)Utility

Method of producing hardened aluminum alloy forming sheet having high strength and superior corrosion resistance

8Forward Citations (#12642265 Global)
0.2/yrCitation Velocity (#31136795 Global)
2.63Citation PageRank (#9363655 Global)
10Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A method of producing a hardened aluminum alloy forming sheet having a high strength and a superior corrosion resistance, the method comprising the steps of (1) providing a melt having a composition consisting of, in weight percentage, 4.0 to 6.0% Mg, 0.05 to 0.50% Cu, 0.10 to 1.0% Mn, 0.01 to 0.05% Ti and the balance being aluminum and impurities; (2) cooling to solidify the melt; (3) hot rolling and cold rolling to form a rolled sheet; and (4) heat treating the rolled sheet by heating to a temperature of 150 DEG to 300 DEG C. at a heating rate of at least 5 DEG C./second, holding within five minutes at the temperature of 150 DEG to 300 DEG C. and cooling to a temperature of 70 DEG C. or less at a cooling rate of at least 30 DEG C./second. The melt may further contain 0.05 to 0.20% by weight Cr and the heat treatment of the step (4) may be carried out under tension after flattening said cold-rolled sheet by leveling at ordinary temperatures. The aluminum alloy sheet is especially suitable for use in manufacturing easy open can ends.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 8.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of producing a hardened aluminum alloy forming sheet having a high strength and a superior corrosion resistance, said method comprising the steps of; (1) providing a melt having a composition consisting of, in weight percentage, Mg: from 4.0 to 6.0%, Cu: from 0.05 to 0.50%, Mn: from 0.10 to 1.0%, Ti: from 0.01 to 0.05% and the balance being aluminum and impurities; (2) cooling to solidify said melt; (3) hot rolling and cold rolling to form a rolled sheet; and (4) heat treating said rolled sheet by heating to a temperature of 150 to 300 ° C at a heating rate of at leas

  2. Claim 2Depends on #1

    A method as claimed in claim 1 in which said melt further conta

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗