Patents
US 4,948,869 A#23326652 Most CitedExpiredUnited States (USPTO)Utility

Molded article of poly (m-phenylene isophthalamide) and process for producing the same

4Forward Citations (#23326652 Global)
0.1/yrCitation Velocity (#43566475 Global)
1.73Citation PageRank (#18325450 Global)
11Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A molded article of poly (m-phenylene isophthalamide), which shows a bending strength of higher than 13 kg/mm 2 , a density of 1.29 to 1.33 g/cm 3 and a Rockwell hardness of not less than M 120 and has an excellent electric insulation and chemical resistance even at a high temperature and a process for producing the same.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 4.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A molded article of poly(m-phenylene isophthalamide) having a bending strength of not less than 13 kg/mm 2 , a density of 1.29 to 1.33 g/cm 3 and Rockwell hardness of not less than M 120.

  2. Claim 2Depends on #1

    The molded article according to claim 1, produced by the steps of drying a poly(m-phenylene isophthalamide) powder having a bulk density of 0.2 to 0.4 g/cm 3 , a specific surface area of 2 to 8 m 2 /g and a mean particle size of 37 to 500 μm to the moisture content of not more than 1% by weight, filling the thus dried poly(m-phenylene isophthalamide) powder into a mold kept at a temperature of not more than 250° C., compressing the thus filled poly(m-phenylene isophthalamide) powder under a pressure of 70 to 500 kg/cm 2 , molding the thus compressed poly(m-phenylene isophthalamide) powd

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗