Abstract

A powder of a rare earth oxide, or a powder of a rare earth oxide and a rare earth metal is mixed with a powder containing iron, a powder containing boron and at least one material selected from among an alkali metal, an alkaline earth metal and a hydrogenated product thereof. The mixture is heated at a temperature of 900 DEG C. to 1200 DEG C. in a non-oxidizing atmosphere, subjected to wet treatment, and heated again at a temperature of 650 DEG C. to 1100 DEG C., whereby an alloy powder is obtained. Alternatively, the mixture is heated at a temperature of 900 DEG C. to 1200 DEG C., crushed into coarse particles, heated again at a temperature of 650 DEG C. to 1100 DEG C. and subjected to wet treatment. The powder is pulverized into a finer powder having an average particle diameter of 1 to 10 microns. The powder is used for making a magnet with a resin.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 3.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for preparing a powder of an alloy of a rare earth element, iron and boron used for making a magnet with a resin, comprising: mixing a powder of a rare earth oxide or a powder of a rare earth oxide and a rare earth metal, a powder containing iron, a powder containing boron, and at least one material selected from the group consisting of an alkali metal, an alkaline earth metal and a hydrogenated product thereof; heating their mixture to a temperature of 900° C. to 1200° C. in a non-oxidizing atmosphere; crushing said mixture coarsely; heating said mixture to a temperature of 65

  2. Claim 2Independent Claim

    A process as set forth in claim

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗