Patents
US 4,937,149 A#5195021 Most CitedExpiredUnited States (USPTO)Utility

Overlay alloy used for a surface layer of sliding material, sliding material having a surface layer comprising said alloy and the manufacturing method of the sliding material

17Forward Citations (#5195021 Global)
0.5/yrCitation Velocity (#17470440 Global)
3.99Citation PageRank (#4776796 Global)
13Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A quaternary overlay bearing alloy used as a surface layer of a sliding bearing consist by weight of Cu in an amount sufficient more than 3% to substantially improve seizure property not more than 6% of Cu, 1-10% of In, not less than 0.1 but less than 5% of Sn, and the balance lead and incidental impurities.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 17.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A composite sliding material comprising a backing metal, a layer of bearing alloy bonded to said backing metal and a surface layer bonded to said layer of bearing alloy, said surface layer being of an alloy consisting, by weight, of Cu of 4 to 4.7%, In of 1 to 10%, Sn not less than 0.1% but less than 5%, and the balance Pb and incidental impurities.

  2. Claim 2Independent Claim

    The composite sliding material as claimed between 6 and 120 μm.

  3. Claim 3Depends on #1

    The composite sliding material as claimed in claim 1 wherein a Cu, Cu-Zn, Cu-Sn, Sn or Ni layer is provided between the layer of the bearing alloy and the surface layer.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • S. Kabra et al., Chemical Abstract No. 99:42055w, "Aluminum-tin Last bearing Alloys", 1983.
  • S. Kabra et al., Chemical Abstract No. 99:42055w, Aluminum tin Last bearing Alloys , 1983.