Stain and scratch resistant resilient surface coverings
Abstract
The present invention relates to surface coverings, and in particular to coverings which comprise treated polyurethane or other wear layers. A coating comprising an aminoplast which is preferably a melamine which is at least partially etherified with alkyl groups comprising 4 to 10 carbon atoms, a vinyl modifier resin, a polyol, and an acid catalyst is formed on a release surface and thermally cured. A crosslinkable wear layer composition is then cast on the cured layer and crosslinked, and the composite is transferred to a support surface. Surface coverings are produced which exhibit surprising resistance to common household stains, and also improved scratch resistance.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 39 · Forward citations: 12.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A surface covering comprising a resilient support and a crosslinked wear layer adhered thereto, the upper portion of the wear layer being formed from a composition comprising: (a) an aminoplast, (b) a vinyl resin, (c) a polyol, (d) a catalyst, and (e) a solvent, the solvent comprising at least 64% by weight of the composition.
- Claim 2Depends on #1
The surface covering of claim 1 wherein the aminoplast is a melamine.
- Claim 3Depends on #2
The surface covering of claim 2 wherein the melamine is alkyl etherified with alkyl groups comprising 1 to 10 carbon atoms.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗