US 4,929,596 A#2615629 Most CitedExpiredUnited States (USPTO)Utility

Process for producing a multiple-filament oxide superconductor

27Forward Citations (#2615629 Global)
0.8/yrCitation Velocity (#9824225 Global)
9.51Citation PageRank (#1153675 Global)
5Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Production of a sheathed wire or multiple-filament conductor composed of ceramic high-temperature superconductor by mixing Y 2 O 3 , CuO and BaO 2 or BaO 2 +BaO, loading the powder mixture (3) into the interior of a metal sheath (1) lined with Ag intermediate layer (2), slowly heating to a maximum permissible reaction/sintering temperature of 950° C. in a period of at least 0.1 h, holding the sintering temperature for at least 1 h, cooling down to 200° C. at at most 10° to 100° C./h to form a conducting core (4) composed of YBa 2 Cu 3 O 6 .5-7.5. Variants having a layer composed of CuO, diffusion barrier composed of Ni, Ta, Nb, V or having Ag intermediate layer doped with AgO or BaO 2 . Preferably reactive sintering under a pressure of 10 to 10.000 bar as hot isostatic pressing. Variant: reactive annealing of the powder mixture under oxygen pressure of 10 to 3000 bar at 600° to 950° C. Pulverizing of the body formed, loading into the metal sheath (1), fabrication, sintering to form a compact superconductor under an external pressure of 10 to 3000 bar at 500° to 900° C. Multiple-filament conductor with centrally arranged tracks of oxygen-releasing substances surrounded by peripheral

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 27.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for producing a multiple-filament oxide superconductor, wherein, at least one group of holes is arranged in a silver body provided with a nickel cladding which serves as a framework, in a manner such that around one central hole in each group there are arranged further holes, and wherein an oxygen-releasing substance whose oxygen saturation vapor pressure is between 10 -3 bar and 2000 bar in a temperature range of 400° to 950° C. selected from the group consisting of BaO 2 ; a mixture of BaO 2 and BaO; MnO 2 ; a mixture of MnO 2 and Mn 2 O 3 ; Pb 3 O 4 ; and a mixture of Pb

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • Advanced Ceramic Materials Ceramic Superconductors, vol. 2, No. 3B, Jul. 1987, Special Supplementary Issue (Westerville, Ohio) pp. 338 340, 471 479, 530 538.
  • Advanced Ceramic Materials--Ceramic Superconductors, vol. 2, No. 3B, Jul. 1987, Special Supplementary Issue (Westerville, Ohio) pp. 338-340, 471-479, 530-538.
  • Japanese Journal of Applied Physics, vol. 26, No. 5, May 1987, pp. 1736 1737, Preparation of High Te . . . Superconductor , T. Kawai, et al.
  • Japanese Journal of Applied Physics, vol. 26, No. 5, May 1987, pp. 1736-1737, "Preparation of High-Te . . . Superconductor", T. Kawai, et al.
  • Japanese Journal of Applied Physics, vol. 26, No. 5, May 1987, pp. 2865 2866, Critical Current . . . Superconductor , S. Nakayama, et al.