US 4,927,718 A#5731530 Most CitedExpiredUnited States (USPTO)Utility

Novel air electrode for metal-air battery with new carbon material and method of making same

16Forward Citations (#5731530 Global)
0.4/yrCitation Velocity (#18169789 Global)
3.11Citation PageRank (#7144803 Global)
10Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A novel carbonaceous electrode support material is disclosed characterized by a corrosion rate of 0.03 wt. %/hour or less when measured a5 550 millivolts vs. a Hg/HgO electrode in a 30 wt. % KOH electrolyte a5 30° C. The electrode support material comprises a preselected carbon black material which has been heat-treated by heating the material to a temperature of from about 2500° to about 3000° C. over a period of from about 1 to about 5 hours in an inert atmosphere and then maintaining the preselected carbon black material at this temperature for a period of at least about 1 hour, and preferably about 2 hours, in the inert atmosphere. A carbonaceous electrode suitable for use as an air electrode in a metal-air cell may be made from the electrode support material by shaping and forming it into a catalyst support and then impregnating it with a catalytically active material capable of catalyzing the reaction with oxygen at the air electrode of metal-air cell.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 16.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A corrosion-resistant carbonaceous electrode support material characterized by a corrosion rate of 0.03 wt.%/hour or less when measured at 550 millivolts vs. a Hg/HgO electrode in a 30 wt.% KOH electrolyte at 30° C., comprising a furnace-process carbon black material which has been heat-treated by heating the material to a temperature of from about 2500° to about 3000° C. over a period of from about 1 to about 5 hours in an inert atmosphere and maintained at this temperature for a period of at least about 1 hour in said inert atmosphere.

  2. Claim 2Depends on #1

    The carbonaceous electrode support material of claim 1 wherein said preselected carbon black material is maintained at said heat treatment temperature from at least about 2 to about 4 hours.

  3. Claim 3Depends on #1

    The carbonaceous electrode support material of claim 1 wherein said preselected ca

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • Kinoshita, Carbon, Electrochemical and Physiochemical Properties ; New York et al, John Wiley and Sons, Inc. 1988, pp. 5 6.
  • Kinoshita, Carbon, Electrochemical and Physiochemical Properties; New York et al, John Wiley and Sons, Inc. 1988, pp. 5≠6.