Abstract
The process for producing crushed zirconium sponge having particle configurations which enhance its compactability, wherein conventionally produced, as-reduced, non-sintered zirconium sponge pieces are loaded into a vacuum furnace, the furnace is heated under partial vacuum at a temperature of up to about 400° C. for a sufficient period to essentially demoisturize and degas the sponge, the temperature is raised to at least about 700° C. and the vacuum terminated, H 2 is fed in a carefully controlled manner into the furnace over a period of several hours in a total amount comprising from about 0.05 to about 0.8% by weight of the sponge, the furnace is cooled, the cooled sponge is pacified, the sponge is removed from the furnace and crushed, the crushed sponge is loaded into a vacuum furnace, the furnace is heated at from about 950° C. to about 1100° C. under partial vacuum for a sufficient period to dehydride the sponge, and the dehydrided sponge, now of enhanced compactability, is cooled and recovered.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 2.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
The process for producing crushed zirconium sponge having particle configurations which enhance its compactability, comprising the steps of: (a) loading as-reduced, non-sintered zirconium sponge pieces into a vacuum furnace; (b) heating said sponge under partial vacuum at a temperature of up to about 400° C. for a sufficient period to essentially demoisturize and degas the sponge; (c) raising the temperature to between about 700° C. and 750° C. and terminating the vacuum; (d) feeding H 2 slowly into the furnace over a predetermined period of time in a total amount of from about 0.05 to
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| FR 2,662,706 A1 | Process for hardening refractory metal sponges | — | 0 |
| US 6,733,563 B2 | Methods for manufacturing hydrogen storage tanks | 2004 | 5 |