Patents
US 4,909,508 A#8854966 Most CitedExpiredUnited States (USPTO)Utility

Golf tees

11Forward Citations (#8854966 Global)
0.3/yrCitation Velocity (#25005603 Global)
3.80Citation PageRank (#5179592 Global)
10Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A golf tee made from peat moss admixed with a water soluble binder in an amount sufficient to bond the peat moss together in a coherent and rigid body by cold or hot pressure forming is disclosed. The water soluble binder may be a lignosulphonate in an amount up to 50%, preferably about 10 to 30%, by weight of the composition. The composition preferably has a moisture content of 5 to 22%, preferably 9 to 18%, by weight. The water soluble binder may be a water soluble polymer in an amount of 3 to 20%, preferably 5 to 15% and more preferably 8 to 10% by weight of the composition.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 11.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of forming golf tees comprising providing a composition of peat moss admixed with a water soluble binder in an amount sufficient to bond the peat moss together in a coherent body and forming said golf tees in a mold under pressure.

  2. Claim 2Depends on #1

    A method as claimed in claim 1 in which said water soluble binder has the characteristics of a binder selected from the group consisting of lignosulphonates and water soluble polymers.

  3. Claim 3Depends on #1

    A method as claimed in claim 1 in which said water soluble binder is a lignosulphonate and said composition comprises by weight up to about 50% lignosulphonates and the balance peat moss containing moisture, and adjusting the moisture content within the range of about 5 to 22% by weight.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗