Process for pulping lignocellulose-containing material
Abstract
A process for the pulping of lignocellulose-containing material, wherein the material is contacted with a pulping medium containing at least 75% by weight of a solvent system, which solvent system comprises from 20 to 95% by weight formic acid; from 5 to 80% by weight of at least one member selected from primary alcohols having from 1 to 3 carbon atoms and esters of formic acid with primary alcohols having from 1 to 3 carbon atoms; and up to 70% by weight of at least one component selected from acetic acid and esters of acetic acid with primary alcohols having from 1 to 3 carbon atoms; and allowing the material to digest at a temperature in ther range of from 140 DEG to 200 DEG C.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 1 · Forward citations: 20.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A process for the pulping of softwood lignocellulose-containing material, wherein the material is contacted with a pulping medium containing at least 90 by weight of a solvent system, which solvent system comprises (a) from 30 to 45% by weight formic acid; (b) from 5 to 15% by weight of methanol or ethanol; and (c) from 40 to 70% by weight of acetic acid; and digesting the material at a temperature in the range of from 160° to 190° C.
- Claim 2Depends on #1
A process as claimed in claim 1, which further comprises the separation of the digestion product into pulp and digest liquor.
- Claim 3Depends on #2
Pulp, whenever prepared by a process as claimed in claim 2.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 20 total)
References Cited — Backward Prior Art (1)
| Patent | Title | Year | Citations |
|---|---|---|---|
| WO 8,201,902 A1 | A process for pulping wood and bark in formic acid | — | 14 |