Abstract

A process for producing a product of carbon fiber reinforced thermoplastic resin comprising immersing carbon fibers in a suspension of a powder of a thermoplastic resin in a liquid medium, which contains at least 20 wt % of an organic liquid and which contains from 0 to 80 wt % water, to impregnate the thermoplastic resin among carbon fibers, and heating the thermoplastic resin deposited on the fibers to melt and form a unitary assembly with carbon fibers.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 1 · Forward citations: 24.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A process for producing a product of carbon fiber reinforced thermoplastic resin comprising immersing carbon fibers in a suspension of a powder of a thermoplastic resin in a liquid medium, which contains at least 20 wt% of an organic liquid which contains from 0 to 80 wt% water, to impregnate the thermoplastic resin among the carbon fibers, and heating the thermoplastic resin deposited on the fibers to melt and form a unitary assembly with carbon fibers.

  2. Claim 2Depends on #1

    A process according to claim 1, wherein the carbon fibers are immersed in the suspension in a form of a strand, a sheet comprising of strands or a fabric comprised of strands.

  3. Claim 3Depends on #2

    A process according to claim 2, wherein the strand comprises of from 12,000 to 10,000,000 filaments.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗