Patents
US 4,895,740 A#20208100 Most CitedExpiredUnited States (USPTO)Utility

Process for manufacturing colored stainless steel wire

5Forward Citations (#20208100 Global)
0.1/yrCitation Velocity (#39268103 Global)
1.65Citation PageRank (#19792208 Global)
20Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A stainless steel wire for springs is proposed which has a colored coating of resinous paint thereon. The wire is coated with a paint, dried and baked to form a coating and is then drawn to a desired diameter. The coating has a good adhesiveness and good heat resistance. The stainless steel wire may be nickel-plated before painting.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 5.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A process for manufacturing a stainless steel wire comprising the steps of applying a colored resinous paint to a thickness of 1 to 500 microns on a stainless steel wire, drying and baking said paint so as to form a coating having a pencil hardness of 6H or less, and cold drawing the coated wire.

  2. Claim 2Depends on #1

    A process as set forth in claim 1, wherein the wire includes a nickel plated layer with a thickness of 1.0 to 15 microns on the wire before coating with the colored resinous paint.

  3. Claim 3Depends on #1

    A process as set forth in claim 1, wherein said coating is heat-resistant so as not to discolor even if heated for annealing for 1 to 60 minutes at a temperature of 200° to 400° C.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (20)