Method of manufacture of glass bodies
Abstract
In a method of manufacturing glass bodies, in which a thixotropic suspension of SiO 2 particles having a diameter in the range from 10 to 500 nm in a dispersing liquid is formed into a green body, after which the green body is purified and sintered, the suspension has a solid:dispersing liquid weight ratio of from 1:1 to 1:1.5, is passed through sieves having an aperture size in the range from 3 to 300 μm under the action of sound or ultrasound, the sieved suspension is then concentrated by pumping off a part of the dispersing liquid under a vacuum and under the influence of sound or ultrasound, such that a solid:dispersing liquid weight ratio of about 1.3:1 is obtained, after which the concentrated suspension is introduced into a mould, heated to a temperature below the boiling point of the dispersing liquid to form a green body. The green body thus obtained is removed from the mould, cooled, and converted to a glass body.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 27.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of manufacturing glass bodies, in which a thixotropic suspension of SiO 2 particles having a diameter in the range from 10 to 500 nm in a dispersing liquid is formed into a green body, after which the green body thus formed is purified and sintered, the method comprising the steps of forming the suspension to have a solid: dispersing liquid weight ratio of from 1:1 to 1:1.5, passing the suspension through at least one sieve having an aperture size in the range from 3 to 300 μm, concentrating the sieved suspension until a solid: dispersing liquid weight ratio of about 1.3:1 is obtaine
Technical Overview & Description