Chemical modification of spin-on glass for improved performance in IC fabrication
Abstract
A process for chemically modifying spin-on-glass (SOG) for improved performance in semiconductor device fabrication is disclosed. To compensate for severe surface topographies associated with very large scale integration (VLSI) technology, a thicker non-etch back SOG process is utilized for forming a SOG layer over a chemical vapor deposition (CVD) layer. A single layer of SOG is formed over the CVD layer, providing planarizing coverage over formational or growth defects. The silylation of the SOG layer provides for the formation thicker single layers of SOG and significantly reduces the wet etching rate in diluted HF.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 126.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A process for silylating spin-on-glass comprising the steps of: depositing a first conductive layer on a semiconductor body; forming said first conductive layer such that openings are created between patterned sections of said first conductive layer; depositing a first dielectric layer on said first conductive layer; depositing a glass layer on said first dielectric layer; annealing said glass layer in an ambient; cooling said semiconductor device in an nitrogen flow bubbled through an organosilicon compound.
- Claim 2Depends on #1
The process as recited in claim 1, wherein said annealing step is in the range of 350°-450° C.
- Claim 3Depends on #2
The process as recited in claim 2, wherein said organo-silicon compound is selected from a group consisting of hexamethyldisilazane (HMDS), dimethyldichlorosilane (DMDCS), trimethylchlorosilane (TMCS), dim
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗