Patents
US 4,882,373 A#529859 Most CitedExpiredUnited States (USPTO)Utility

Asphaltic composition

67Forward Citations (#529859 Global)
1.8/yrCitation Velocity (#2492148 Global)
16.23Citation PageRank (#473602 Global)
6Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

An asphaltic composition having improved tensile properties is disclosed. Also disclosed is a method for producing said composition which comprises: A. contacting an asphalt with a mineral acid; B. contacting the acid modified asphalt thus formed with an oxygen-containing gas; C. adding a thermoplastic elastomer to the acid/oxygen modified asphalt thus formed; and D. adding an unsaturated functional monomer to the polymer modified asphalt. In a preferred embodiment, the asphalt is contacted with an oxygen-containing gas prior to and during contact with the mineral acid.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 67.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    An asphaltic composition having improved tensile properties that is produced by the method comprising: (a) contacting asphalt with from about 0.25 to about 4 wt. % of a mineral acid to form an acid modified asphalt, (b) contacting said acid modified asphalt with an oxygen-containing gas to form an acid/oxygen modified asphalt, the temperature of the asphalt during said contacting in (a) and (b) being maintained between about 200° C. and about 300° C., (c) contacting said acid/oxygen modified asphalt with from about 5 to about 25 wt. % of a thermoplastic elastomer at a temperature between a

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • Abstract of Japanese Patent 56 115354, 9/81.
  • Abstract of Japanese Patent 56-115354, 9/81.